Characterization of pitting corrosion damage through multiscale analysis

G. N. Frantziskonis, L. B. Simon, J. Woo, T. E. Matikas

Research output: Contribution to journalConference articlepeer-review

1 Scopus citations

Fingerprint

Dive into the research topics of 'Characterization of pitting corrosion damage through multiscale analysis'. Together they form a unique fingerprint.

Mathematics

Physics & Astronomy

Engineering & Materials Science